Pressure points and scratches in solid wood, such as those used in parquet floors and high-quality furniture, are indeed annoying but easy to eradicate. The special properties of solid wood-based materials make it possible to remedy the situation with relatively simple repair options even as home improvement. In this article, the common methods for wood repair and repair are shown and explained.

Repair solid wood with heat and moisture

Solid wood is a one hundred percent natural product and has one resilient and permeable to air and water permeable cell and fiber structure. Even wood built into furniture works and "lives on" in a way: through heat and cold, moisture and dryness, the wood contracts and widens. This usually goes unnoticed. Only at extreme values, these strains are expressed by clamping cabinet doors and sliding drawers.

Small damage to the wood by dents are therefore even without household aids usually removable. Moisture and heat cause the wood fibers to expand and return to their original, smooth shape. An iron and a damp cloth are enough for this: The iron is adjusted to wool warmth, this is usually the first stage. Then the damp cloth is placed on the damaged area and heated with the iron, it should not be rubbed. Then the dent may have disappeared, otherwise this technique can be used several times. Usually this is enough to eliminate the damage.

Remove damage with wax: this is needed

  • Wood repair set (mostly consisting of different colored waxes)
  • Fine sandpaper for wood (grit 180-220)
  • Iron
  • Fleece or molton cloth
  • possibly parquet sealing in parquet floors (clearcoat)

Repair dents, holes and scratches with wax

Repair wood scraper and repair wood: repair

Damage in the wood

Every better assorted hardware store has solid wood repair kits ready for you. Most of these consist of one or more small blocks of wax, which should cover the damaged area merging with the surrounding wood. For professionals, this method of removing damage and bruises in the wood is the first choice. However, do-it-yourselfers sometimes have problems: dealing with the wax needs to be learned, and it is not unusual for the repair site to be more visible than desired in the end.

Often this is due to a lack of preparation: Regardless of whether the spot is on parquet or solid wood furniture: First, the old seal or the oiled surface must be removed with fine sandpaper.

Repair wood scraper and repair wood: wood

Waxing in the damage

For this purpose, the surface around the damaged area is first processed with a little coarse sandpaper (grit 180) and then smoothed with 220 grit. Any splinters around the damaged area must be carefully removed, the edges of the crack or the dent should be as smooth as possible.

Subsequently will warmed up the repair wax. If necessary, this can be done with the body heat of the palm, it is better to put the wax on a pad in the oven at 50° C for about 10 minutes. So it becomes supple for the repair.

Repair wood scraper and repair wood: scratches

Grind damaged area

The heated wax is then added "incorporated" into the damaged area. It is important to ensure that the damage is really completely filled with wax. Supernatants are not bad.

Now will the iron is heated to wool temperature and place the cloth or fleece over the damaged area. Several times now is ironed - always the course of the wax should be checked in between. In case of doubt prefer to add some wax and iron again - the place must be completely filled.

When everything is filled, the wax must first cool. For this should about an hour to be calculated. Then the repair site is sanded again with the fine sandpaper. Finally, either the parquet seal or new furniture oil applied - finished is the (almost) invisible solid wood repair.

Remove scratches and dents from plywood

Similar to how solid wood can be repaired with wax, veneer wood can also be repaired. The advantage here is, however, if the veneer imitates real wood and thus already contains color differences. So repair sites are not very noticeable, but it always depends on the size. The procedure is basically the same as the procedure above, however, veneer may not be sanded. Excess wax residues must therefore already be removed by the ironing procedure or with a sharp Ceranfeldschaber.

The repair job is less stable in veneer, because the wax can not penetrate into the surrounding wood. Nevertheless, for example, when installing new door handles on room doors, the use of wax for lamination of old screw holes first choice.

Similar sites

  • Jigsaw templates
  • Remove candle wax
  • Remove scratches - exterior mirror housings
  • Tinker with wood
  • Wood surfaces treat with oil, wax, varnish and glaze
  • Repair laminate - repair scratches in the laminate
  • Remove the rust
  • Repair patio tiles and repair patio tiles
  • Brushing instructions: Remove paint with paint stripper
  • Repair and repair concrete damage
  • Repair / restore the speaker
  • Denting: Dents remove - Dentists in their own right
  • Restore furniture: pickle, repair and paint
  • Renovate wooden staircase
  • Remove rust stains

Video Board: How to Fix Rotted Wood with Epoxy - This Old House